Material Notes:
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.31 - 1.37 g/cc
1.31 - 1.37 g/cc
ASTM D 792
ASTM Color -1.31 - 4.69
-1.31 - 4.69
Color A, ME 12
3.54 - 9.54
3.54 - 9.54
Color B, ME 12
67.56 - 73.56
67.56 - 73.56
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore D 78 - 82

@Time 15.0 sec
78 - 82

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 53.9 MPa
>= 7820 psi
ASTM D 638
Descriptive Properties Value Comments
Application General Purpose Injection Molded Parts