Karina 800-DA-10/1-A-AT-IS White PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Extruded
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina 800-DA-10/1-A-AT-IS White PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.29 - 1.35 g/cc
1.29 - 1.35 g/cc
ASTM D 792
ASTM Color -2.01 - 0.99
-2.01 - 0.99
Color A, ME 12
0.99 - 3.99
0.99 - 3.99
Color B, ME 12
90.02 - 93.02
90.02 - 93.02
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 80 - 84

@Time 15.0 sec
80 - 84

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 13.7 MPa
>= 1990 psi
ASTM D 638
Elongation at Break >= 250 %
>= 250 %
ASTM 638
Descriptive Properties Value Comments
Application Lavatory Drain Hose