Karina 740-DA-18/339-A-IS-BZ Gray PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina 740-DA-18/339-A-IS-BZ Gray PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Heavy metal free PVC compound recommended for injection of automotive parts.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.22 - 1.28 g/cc
1.22 - 1.28 g/cc
ASTM D 792
ASTM Color -2.96 - -1.96
-2.96 - -1.96
Color B, ME 12
-0.560 - 0.44
-0.560 - 0.44
Color A, ME 12
29.33 - 30.33
29.33 - 30.33
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 72 - 76

@Time 15.0 sec
72 - 76

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 13.7 MPa
>= 1990 psi
ASTM D 638
Elongation at Break >= 280 %
>= 280 %
ASTM D 638
Component Elements Properties Metric English Comments
Cadmium, Cd <= 0.0050 %
<= 0.0050 %
IEC 62321
Chromium, Cr <= 0.010 %
<= 0.010 %
IEC 62321
Lead, Pb <= 0.010 %
<= 0.010 %
IEC 62321
Mercury, Hg <= 0.010 %
<= 0.010 %
IEC 62321
Descriptive Properties Value Comments
Application Automotive
Bromine, Br (%) < 0.01
IEC 62321