Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Karina 700D40/356-AT Green PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina 700D40/356-AT Green PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Non toxic PVC compound, recommended for injection of inhalation maskInformation provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.17 - 1.21 g/cc
1.17 - 1.21 g/cc
ASTM D 792
ASTM Color -7.96 - -1.96
-7.96 - -1.96
Color A, ME 12
-1.72 - 4.28
-1.72 - 4.28
Color B, ME 12
83.5 - 89.5
83.5 - 89.5
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 68 - 72

@Time 15.0 sec
68 - 72

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 9.32 MPa
>= 1350 psi
ASTM D 638
Elongation at Break >= 200 %
>= 200 %
ASTM D 638
Tear Strength >= 40.0 kN/m
>= 228 pli
DIN 53507
Abrasion <= 200
<= 200
mm<sup>3</sup>; DIN 53516
Descriptive Properties Value Comments
Application Inhalation Masks
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved