Karina 651D10/1-C-IS White PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina 651D10/1-C-IS White PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.27 - 1.33 g/cc
1.27 - 1.33 g/cc
ASTM D 792
ASTM Color -1.92 - 1.08
-1.92 - 1.08
Color A, ME 12
-0.650 - 2.35
-0.650 - 2.35
Color B, ME 12
92.01 - 95.01
92.01 - 95.01
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 63 - 67

@Time 15.0 sec
63 - 67

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 9.81 MPa
>= 1420 psi
ASTM D 638
Elongation at Break >= 300 %
>= 300 %
ASTM D 638
Descriptive Properties Value Comments
Application General Purpose Accessories