Karina 603-48/1-Y-BZ Black PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina 603-48/1-Y-BZ Black PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
For footware.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.22 - 1.28 g/cc
1.22 - 1.28 g/cc
ASTM D 792
ASTM Color -1.38 - 0.22
-1.38 - 0.22
Color B, ME 12
-0.860 - 0.74
-0.860 - 0.74
Color A, ME 12
25.96 - 27.56
25.96 - 27.56
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 58 - 62

@Time 15.0 sec
58 - 62

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 7.85 MPa
>= 1140 psi
ASTM D 638
Elongation at Break >= 200 %
>= 200 %
ASTM D 638
Tear Strength >= 25.0 kN/m
>= 143 pli
DIN 53507
Abrasion <= 265
<= 265
mm<sup>3</sup>; DIN 53516