Karina 600D48/1-C-IS Black PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Extruded , PVC, Molded
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina 600D48/1-C-IS Black PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PVC Compound recommended for injection of automotive parts and extrusion of flexible jacket for electrical cablesInformation provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.28 - 1.32 g/cc
1.28 - 1.32 g/cc
NBR NM-IEC 60811-1-3
ASTM Color -1.36 - 0.24
-1.36 - 0.24
Color B, ME 12
-0.780 - 0.82
-0.780 - 0.82
Color A, ME 12
25.07 - 26.67
25.07 - 26.67
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 58 - 62

@Time 15.0 sec
58 - 62

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 7.85 MPa
>= 1140 psi
ASTM D 638
Elongation at Break >= 250 %
>= 250 %
ASTM D 638
Descriptive Properties Value Comments
Application Automotive