Karina 02/223-G Yellow Color Concentrate for PVC

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina 02/223-G Yellow Color Concentrate for PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Color concentrate recommended for application in PVC compounds for general purposes injection. Recommended to use 2%.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.26 - 1.30 g/cc
1.26 - 1.30 g/cc
NBR NM-IEC 60811-1-3
ASTM Color -26.16 - -23.16
-26.16 - -23.16
Color A, ME 12
79.33 - 82.33
79.33 - 82.33
Color B, ME 12
88.18 - 91.18
88.18 - 91.18
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 68 - 72

@Time 15.0 sec
68 - 72

@Time 0.00417 hour
ASTM D 2240
Descriptive Properties Value Comments
Application Injection