KaMin Hydralux® 91 Clay

Category Ceramic , Clay
Manufacturer KaMin LLC
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF KaMin Hydralux® 91 Clay.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hydralux® 91 is a high brightness, fine glossing coating clay used in heavy weight coated paper and coated board application. Its fine particle excellent flow properties and size allow for high solids coating and provide excellent glossing properties.Industry: PAPER & PACKAGINGUses: Coated Freesheet/Art Paper, Coated 1S Label, Coated Bleached Board, Coated Recycle Board, Coated Natural Kraft, Thermal PaperInformation provided by KaMin LLC.
Physical Properties Metric English Comments
Solids Content 69.5 - 71 %
69.5 - 71 %
Slurry
Brightness 88.5 - 90.5 %
88.5 - 90.5 %
ISO
91 - 92.5 %
91 - 92.5 %
Reflectance (TAPPI)
Moisture Absorption at Equilibrium <= 1.5 %
<= 1.5 %
As Produced
Particle Mesh Size 325 Mesh
325 Mesh
0.005% Retained
pH 6 - 8
6 - 8
100 g/250 ml H2O Slurry
Brookfield Viscosity 500 cP

@Temperature 25.0 °C
500 cP

@Temperature 77.0 °F
20 RPM
Descriptive Properties Value Comments
CAS Number 1332-58-7
Physical Forms Dry, Slurry
Shipping Point Wrens, GA