Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

KYDEX® XDWG 3D Laminate Capped Woodgrain Thermoplastic Sheet for Flat Lamination and Membrane Pressed Uses

Category Polymer , Thermoplastic
Manufacturer KYDEX LLC
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF KYDEX® XDWG 3D Laminate Capped Woodgrain Thermoplastic Sheet for Flat Lamination and Membrane Pressed Uses.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features:Tough and durableResistant to cracking and chippingSolid, integral colorAvailable in a variety of wood grain designsMatched to popular high pressure laminates and melaminesResistant to a wide range of chemicalsAbrasion resistantFire retardantExcellent fabrication qualitiesVery low moisture absorptionMembrane pressableFlexibility allows small radius bendsSuggested Applications:Store fixturesCheckout countersExhibits and displaysMoldingsTransaction surfacesWorkstationsLogo and trademark panelsKiosksCabinetryDoor and drawer fasciasPedestals and standsTabletopsFlat laminated panelsInformation provided by Kydex, LLC.
Descriptive Properties Value Comments
Ball Impact Resistance > 3000 mm
NEMA LD3.8
Cleanability 14
NEMA LD3.4
No Effect
NEMA LD3.4; 1-2, 4-15
Severe Effect
NEMA LD3.4; 3
Dart Impact Resistance > 875 mm
NEMA LD3.9
Surface Burning Characteristics: Flame Spread/Smoke Class 1/A
ASTM E84
Wear Resistance 650 cycles
NEMA LD3.13