KYDEX® XD MB 3D Laminate Thermoplastic 3D Laminate for Flat Lamination and Membrane Pressed Uses with Microban®

Category Polymer , Thermoplastic
Manufacturer KYDEX LLC
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF KYDEX® XD MB 3D Laminate Thermoplastic 3D Laminate for Flat Lamination and Membrane Pressed Uses with Microban®.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features:Tough and extremely durableResistant to cracking and chippingSolid, integral color4,000+ custom colorsResistant to a wide range of chemicalsAbrasion resistantFire retardantVery low moisture absorptionMembrane pressableFlexibility allows small radius bendsMicroban® antimicrobial technology inhibits the growth of bacteria that can cause stains, odors and product deterioration.Microban® technology is built-in to the sheet so it won't wash or wear away and lasts for the lifetime of the product.Microban® technology keeps the surface cleaner between cleanings.Suggested Applications:Store fixturesCheckout countersExhibits and displaysMoldingsTransaction surfacesWorkstationsLogo and trademark panelsKiosksCabinetryDoor and drawer fasciasPedestals and standsGondolasTabletopsFlat laminated panelsInformation provided by Kydex, LLC.
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 94
94
ASTM D785
Tensile Strength 42.0 MPa
6090 psi
ASTM D638
Elongation at Break 126 %
126 %
ASTM D638
Tensile Modulus 2.416 GPa
350.4 ksi
ASTM D638
Flexural Strength 66.0 MPa
9570 psi
ASTM D790
Flexural Modulus 2.48 GPa
360 ksi
ASTM D790
Izod Impact, Notched 8.01 J/cm
15.0 ft-lb/in
ASTM D256
Taber Abrasion, mg/1000 Cycles 9.5
9.5
CS10F wheel, 500 g load; ASTM D1044
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 66.2 °C
151 °F
unannealed; ASTM D648
75.6 °C
168 °F
annealed; ASTM D648
Descriptive Properties Value Comments
Ball Impact Resistance > 3000
NEMA LD3 - 2005
Cleanability 16
NEMA LD3 - 2005
Dart Impact Resistance > 1000
NEMA LD3 - 2005