KYDEX® 5555 Low Heat Release Aviation Thermoforming Sheet

Category Polymer , Thermoplastic
Manufacturer KYDEX LLC
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF KYDEX® 5555 Low Heat Release Aviation Thermoforming Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features:Over two hundred colors and eight thicknesses availableChemical resistantMeets flamespread and smoke density requirements for mass transitSuggested Applications:Seat partsBulkhead laminatesLife vest shroudsPassenger service unitsMonitor shroudsArmrestsWindow shadesMolding stripsTray tablesKick panelsInformation provided by Kydex, LLC.
Physical Properties Metric English Comments
Specific Gravity 1.52 g/cc
1.52 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 111
111
ASTM D785
Tensile Strength 43.0 MPa
6240 psi
ASTM D638
Flexural Strength 81.2 MPa
11800 psi
ASTM D790
Flexural Modulus 3.833 GPa
555.9 ksi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 75.9 °C
169 °F
annealed; ASTM D648
Processing Properties Metric English Comments
Processing Temperature 170 - 200 °C
338 - 392 °F
Forming
Descriptive Properties Value Comments
Federal Aviation Administration < 150
FAR 25.853 (d); Smoke Generation
< 55/55
FAR 25.853 (d); Rate of Heat Release
Pass
FAR 25.853 (a)