Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

KKPC Kuhmo HF400 Flame Retarded General Purpose HIPS

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Flame Retardant
Manufacturer Korea Kumho Petrochemical Co., Ltd.
Trade Name Kuhmo
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF KKPC Kuhmo HF400 Flame Retarded General Purpose HIPS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key features: Translucent Injection. Common Uses: TV and VCR housing.HIPS is a functional resin made by copolymerization of styrene monomer and PBR. It shows excellent balance between impact-resistance and heat-resistance.Data provided by Korea Kumho Petrochemical Co., Ltd.
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
ASTM D792
Water Absorption 0.050 %
0.050 %
24 hr immersion; ASTM D570
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
ASTM D955
Melt Flow 12 g/10 min
12 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 55
55
ASTM D785
Tensile Strength, Ultimate 24.5 MPa
3560 psi
ASTM D638
Elongation at Break 70 %
70 %
ASTM D638
Flexural Yield Strength 43.2 MPa
6260 psi
ASTM D790
Flexural Modulus 1.96 GPa
284 ksi
ASTM D790
Izod Impact, Notched 1.33 J/cm

@Thickness 3.20 mm
2.50 ft-lb/in

@Thickness 0.126 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 76.0 °C
169 °F
annealed; ASTM D648
85.0 °C
185 °F
unannealed; ASTM D648
Vicat Softening Point 94.0 °C
201 °F
ASTM D1525
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
V-0

@Thickness 3.20 mm
V-0

@Thickness 0.126 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Strength 17.7 kV/mm
450 kV/in
ASTM D149