Johnson Matthey SW 850 Platinum w/ 15% Iridium Jewelry Alloy

Category Metal , Nonferrous Metal , Precious Metal , Platinum Alloy
Manufacturer Johnson Matthey
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Johnson Matthey SW 850 Platinum w/ 15% Iridium Jewelry Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Springs, watch backs. Copper, cobalt, gold, iridium, palladium and ruthenium alloy easily with platinum. The differences between the alloys reflect the hardening of the alloying element itself.
Physical Properties Metric English Comments
Density 21.5 g/cc
0.777 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 160
160
Annealed
Elongation at Break 15 %
15 %
Annealed
Thermal Properties Metric English Comments
Melting Point 1800 - 1820 °C
3270 - 3310 °F
Solidus 1800 °C
3270 °F
Liquidus 1820 °C
3310 °F
Component Elements Properties Metric English Comments
Iridium, Ir 15 %
15 %
Platinum, Pt 85 %
85 %