Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Johnson Matthey Argo-braze 40N Silver Brazing Alloy for Tungsten Carbide Brazing

Category Metal , Nonferrous Metal , Precious Metal , Silver Alloy , Solder/Braze Alloy
Manufacturer Johnson Matthey
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Johnson Matthey Argo-braze 40N Silver Brazing Alloy for Tungsten Carbide Brazing.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
An economical alloy for brazing tungsten carbides and stainless steels. Optimum Joint Gap 0.1 - 0.25 mm.AWS A5.8-92 BAg-4Federal Specification QQ-B-564 BAg-4Information provided by Johnson Matthey.
Thermal Properties Metric English Comments
Melting Point 660 - 780 °C
1220 - 1440 °F
Solidus 660 °C
1220 °F
Liquidus 780 °C
1440 °F
Component Elements Properties Metric English Comments
Copper, Cu 30 %
30 %
Nickel, Ni 2.0 %
2.0 %
Silver, Ag 40 %
40 %
Zinc, Zn 28 %
28 %