Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

JPJ Technologies HDPE Pipe Grade

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Pipe Grade
Manufacturer JPJ Technologies
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF JPJ Technologies HDPE Pipe Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by JPJ Technologies
Physical Properties Metric English Comments
Density 0.949 g/cc
0.0343 lb/in³
GB 1033
Melt Flow 0.10 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.10 g/10 min

@Load 4.76 lb,
Temperature 374 °F
GB3682
0.50 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.50 g/10 min

@Load 11.0 lb,
Temperature 374 °F
GB3682
Mechanical Properties Metric English Comments
Tensile Strength at Break 33.0 MPa
4790 psi
GB1040
Tensile Strength, Yield 22.0 MPa
3190 psi
GB1040
Elongation at Break 800 %
800 %
GB1040
Tensile Modulus 0.800 GPa
116 ksi
GB1040
Charpy Impact, Notched NB
NB
ISO 179
Descriptive Properties Value Comments
Thermal stability 50 min
@ 210°C, ISO10837
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved