JPJ Technologies 3000j/JE HDPE Injection

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer JPJ Technologies
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF JPJ Technologies 3000j/JE HDPE Injection.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by JPJ Technologies
Physical Properties Metric English Comments
Density 0.957 g/cc
0.0346 lb/in³
Melt Flow 2.3 g/10 min
2.3 g/10 min
Mechanical Properties Metric English Comments
Tensile Strength at Break 26.0 MPa
3770 psi
Elongation at Break 400 %
400 %