JPJ Technologies 2200J HDPE Injection

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer JPJ Technologies
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF JPJ Technologies 2200J HDPE Injection.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by JPJ Technologies
Physical Properties Metric English Comments
Density 0.964 g/cc
0.0348 lb/in³
Melt Flow 5.5 g/10 min
5.5 g/10 min
Mechanical Properties Metric English Comments
Tensile Strength at Break 23.0 MPa
3340 psi
Elongation at Break 180 %
180 %