Isoflon Teflon® 20 AD Polytetrafluoroethylene Film

Category Polymer , Film , Thermoplastic , Fluoropolymer , PTFE
Manufacturer Isoflon
Trade Name Teflon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Isoflon Teflon® 20 AD Polytetrafluoroethylene Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Adhesive Skived Pure PTFE FilmInformation provided by Isoflon.
Physical Properties Metric English Comments
Thickness 50.0 microns
1.97 mil
Adhesive
500 microns
19.7 mil
Backing
Coating Weight 1080 g/m²
675 lb/ream
Film Weight; NF EN ISO 2286.2
Mechanical Properties Metric English Comments
Elongation at Break >= 200 %
>= 200 %
Tear Strength 8.80 kN/m
50.2 pli
Peel Strength 0.720 kN/m
4.11 pli