Isoflon Polyester Mesh

Category Polymer , Thermoplastic , Polyester, TP
Manufacturer Isoflon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Isoflon Polyester Mesh.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Open mesh polyester, 1 x 1 mm, is used in a large number of industries such as food processing, textiles, packaging and electronics for single filtration or for drying ovens.Thanks to its great flexibility, this fabric provides the advantage of being able to be wound on small reel diameters.Good chemical resistance.Information provided by Isoflon.
Physical Properties Metric English Comments
Bulk Density 0.500 g/cc
0.0181 lb/in³
Filament Diameter 500 µm

@Thickness 0.900 mm
500 µm

@Thickness 0.0354 in
Nominal weight 450 g/m²
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
100°C in humid environments
Descriptive Properties Value Comments
Color White