Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Isoflon PETP Polyethylene terephthalate

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer Isoflon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Isoflon PETP Polyethylene terephthalate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Good optical propertiesHigh UV resistanceAbsorbs little moistureInformation provided by Isoflon.
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
DIN 53479
Water Absorption 0.25 %
0.25 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell M 96
96
ASTM D785
Tensile Strength 80.0 MPa
11600 psi
DIN 53455
Elongation at Break 10 %
10 %
DIN 53455
Tensile Modulus 3.00 GPa
435 ksi
DIN 53457
Thermal Properties Metric English Comments
CTE, linear 70.0 µm/m-°C
38.9 µin/in-°F
DIN 52328
Thermal Conductivity 0.290 W/m-K
2.01 BTU-in/hr-ft²-°F
DIN 52612
Melting Point 255 °C
491 °F
DIN 53736
Maximum Service Temperature, Air 100 °C
212 °F
Continuous; DIN 52612
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
212 °F
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Continuous; DIN 52612
Flammability, UL94 V-2
V-2
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
DIN 53482
Dielectric Constant 3.3

@Frequency 1000 Hz
3.3

@Frequency 1000 Hz
DIN 53483
Dielectric Strength 25.0 - 85.0 kV/mm
635 - 2160 kV/in
DIN 53481