Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Isoflon PA 6G Cast Polyamide 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Cast
Manufacturer Isoflon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Isoflon PA 6G Cast Polyamide 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General use for mechanical partsGood heat resistanceEasy to useHigh moisture regainInformation provided by Isoflon.
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
DIN 53479
Water Absorption 2.0 %
2.0 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 112
112
ASTM D785
Tensile Strength 75.0 MPa
10900 psi
DIN 53455
Elongation at Break 60 %
60 %
DIN 53455
Tensile Modulus 2.40 GPa
348 ksi
DIN 53457
Thermal Properties Metric English Comments
CTE, linear 75.0 µm/m-°C
41.7 µin/in-°F
DIN 52328
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
DIN 52612
Melting Point 220 °C
428 °F
DIN 53736
Maximum Service Temperature, Air 100 °C
212 °F
Continuous; DIN 52612
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C
203 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Continuous; DIN 52612
Flammability, UL94 V-2
V-2
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
DIN 53482
Dielectric Constant 3.7

@Frequency 1000 Hz
3.7

@Frequency 1000 Hz
DIN 53483
Dielectric Strength 19.0 - 29.0 kV/mm
483 - 737 kV/in
DIN 53481
Descriptive Properties Value Comments
Color Nat.
Users viewing this material also viewed the following: