Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Iran Petrochemical (PCC) Tabriz 0640AA LLDPE  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Film Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) Tabriz 0640AA LLDPE  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.928 - 0.932 g/cc
0.0335 - 0.0337 lb/in³
ASTM D792
Melt Flow 3.8 - 4.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.8 - 4.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 12.0 MPa
1740 psi
ISO 1184
Film Tensile Strength at Yield, TD 12.0 MPa
1740 psi
ISO 1184
Film Elongation at Break, MD >= 785 %
>= 785 %
ISO 1184
Film Tensile Strength at Break, MD >= 33.0 MPa
>= 4790 psi
ISO 1184
Film Tensile Strength at Break, TD 25.0 MPa
3630 psi
ISO 1184
Thermal Properties Metric English Comments
Vicat Softening Point >= 104 °C
>= 219 °F
ASTM D1525
Users viewing this material also viewed the following: