Iran Petrochemical (PCC) Tabriz 0410AA LLDPE  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Film Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) Tabriz 0410AA LLDPE  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.924 - 0.928 g/cc
0.0334 - 0.0335 lb/in³
B.P. 125
Melt Flow 0.90 - 1.1 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.90 - 1.1 g/10 min

@Load 4.76 lb,
Temperature 374 °F
B.P. 112
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD >= 12.0 MPa
>= 1740 psi
Film Tensile Strength at Yield, TD >= 13.0 MPa
>= 1890 psi
Film Elongation at Break, MD >= 650 %
>= 650 %
Film Elongation at Break, TD >= 850 %
>= 850 %
Dart Drop Test >= 80.0 g
>= 0.176 lb
Film Tensile Strength at Break, MD >= 42.0 MPa
>= 6090 psi
Film Tensile Strength at Break, TD >= 33.0 MPa
>= 4790 psi
Thermal Properties Metric English Comments
Vicat Softening Point >= 105 °C
>= 221 °F
At 1 kg
Descriptive Properties Value Comments
Whiteness Index >48