Iran Petrochemical (PCC) TPC - 221 HS Expandable Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Molded, Unreinforced
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) TPC - 221 HS Expandable Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TPC - 221 HSApplication: low to medium density blocksInformation provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.0140 - 0.0300 g/cc
0.000506 - 0.00108 lb/in³
Final Product Density
Bead Size 1.00 - 1.80 mm
0.0394 - 0.0709 in