Iran Petrochemical (PCC) SH-0150 Acrylonitrile Butadiene Styrene

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) SH-0150 Acrylonitrile Butadiene Styrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SH - 0150 ABS extrusion grade has been formulated to provide excellent mechanical properties,extrusion stability, vacuum formability and chemical resistance. It is a high flow extrusion grade with high impact strength at ambient temperature and considerable impact strength at low temperatures. This grade has a wide processing window.Applications: parts with significant impact resistance, general sheets.Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
ASTM D955
Melt Flow 1.1 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.1 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 106
106
ASTM D785
Tensile Strength, Yield 44.1 MPa
6400 psi
ASTM D638
Flexural Yield Strength 63.7 MPa
9250 psi
ASTM D790
Flexural Modulus 2.21 GPa
321 ksi
ASTM D790
Izod Impact, Notched (ISO) 28.0 kJ/m²
13.3 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Vicat Softening Point 101 °C
214 °F
ASTM D1525
Flammability, UL94 HB
HB