Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Iran Petrochemical (PCC) Moplen EP-YS30RE Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Extrusion Grade
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name Moplen
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) Moplen EP-YS30RE Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Moplen EP-YS30RE is a heterophasic polypropylene copolymer designed for extrusion applications where smooth processability and a good balance of mechanical properties are required. Moplen EP-YS30RE offers excellent processability and the final items show good stiffness and outstanding impact resistance, even at temperatures down to -20°C.Applications: sheet for thermoforming, corrugated board, blow molded bottles and containers for detergents.Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ISO 1183
Melt Flow 1.3 g/10 min
1.3 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 64
64
ISO 868
Tensile Stress 27.0 MPa
3920 psi
ISO R527
Elongation at Yield 13 %
13 %
ISO R527
Flexural Modulus 1.10 GPa
160 ksi
ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Vicat Softening Point 151 °C
304 °F
ISO 306/A
Heat Distortion Temperature 88.0 °C

@Pressure 0.460 MPa
190 °F

@Pressure 66.7 psi
ISO 75/B