Iran Petrochemical (PCC) Moplen EP-S31HP Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Extrusion Grade
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name Moplen
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) Moplen EP-S31HP Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Moplen EP-S31HP is a heterophasic polypropylene copolymer with an exceptional mechanical properties balance. In comparison with standard polypropylene copolymers with the same fluidity, Moplen EP-S31HP offers some distinct advantages: higher stiffness, superior impact resistance both at room temperature and at low temperatures, excellent creep and deformation resistance, very high dimensional stability.Applications: baler twines, packaging twines and ropes, brush and broom filling and technical applications.Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ISO 1183
Melt Flow 6.0 g/10 min
6.0 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 71
71
ISO 868
Tensile Stress 34.0 MPa
4930 psi
ISO R527
Elongation at Yield 13 %
13 %
ISO R527
Flexural Modulus 1.50 GPa
218 ksi
ISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²
1.90 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Vicat Softening Point 155 °C
311 °F
ISO 306/A
Heat Distortion Temperature 119 °C
246 °F
ISO 75/B