Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Iran Petrochemical (PCC) GPPS 1540 Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Extrusion Grade , Polystyrene, Molded, Unreinforced
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) GPPS 1540 Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
GPPS 1540 is an easy flowing crystal polystyrene designed for extrusion or injection applications. In extrusion, it improves extruder output and thermoforming cycle times when mixed with a high impact polystyrene. It is particularly suitable for glossy-layer co-extrusion.Applications: impact dilution, gloss layer in co-extrusion, packaging articles, medical applications, office equipmentInformation provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
Moisture Absorption <= 0.100 %
<= 0.100 %
ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
ASTM D570
Melt Flow 11 g/10 min

@Load 5.00 kg,
Temperature 200 °C
11 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 45.0 MPa
6530 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Tensile Modulus 3.10 GPa
450 ksi
ASTM D638
Flexural Modulus 3.00 GPa
435 ksi
ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point >= 89.5 °C
>= 193 °F
ASTM D1525
Optical Properties Metric English Comments
Refractive Index 1.591
1.591
ISO