Iran Petrochemical (PCC) EX 2 HF 7750 M High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , HDPE, Fiber Grade
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) EX 2 HF 7750 M High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EX2 is a high density polyethylene with 1-Butene as co monomer. It has good rigidity and medium molar mass. Applications: monofilaments, ropes, yarns.Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.956 g/cc
0.0345 lb/in³
ISO 1183
Melt Flow 2.5 g/10 min

@Load 5.00 kg,
Temperature 190 °C
2.5 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
25 g/10 min

@Load 21.6 kg,
Temperature 190 °C
25 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 59
59
ISO 868
Tensile Stress 31.0 MPa
4500 psi
at Break; ISO 527
Tensile Strength, Yield 27.0 MPa
3920 psi
ISO 527
Elongation at Break >= 1000 %
>= 1000 %
ISO 527
Elongation at Yield 10 %
10 %
ISO 527
Tensile Modulus 1.20 GPa
174 ksi
ISO 527
Charpy Impact, Notched 1.90 J/cm²
9.04 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Softening Point 80.0 °C
176 °F
ISO 306
Brittleness Temperature >= -80.0 °C
>= -112 °F
ASTM D746-72
Processing Properties Metric English Comments
Melt Temperature 220 - 270 °C
428 - 518 °F
Descriptive Properties Value Comments
Flexural Creep Modulus (MPa) 1350
4 point, 1 min; DIN 19537-2