Iran Petrochemical (PCC) 7000F High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Film Grade
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) 7000F High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
7000F is a high density polyethylene for enhanced ultra thin film.Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.952 g/cc
0.0344 lb/in³
ISO 1183
Melt Flow 0.040 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.040 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Stress 38.2 MPa
5540 psi
at Break; ASTM D1238
Tensile Strength, Yield 24.5 MPa
3550 psi
ASTM D1238
Elongation at Break >= 500 %
>= 500 %
ASTM D638
Processing Properties Metric English Comments
Melt Temperature 131 °C
268 °F