Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Iran Petrochemical (PCC) 6070EA High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) 6070EA High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HD6070EA is a high density polyethylene with a narrow molecular weight distribution. It is suitable for a wide range of injection molding applications. This grade has following characteristics: easy processing, high rigidity, good impact strength, and high warpage resistance.Applications: crates, boxes, seatsInformation provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.960 g/cc
0.0347 lb/in³
ASTM D1505
Melt Flow 7.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
7.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 68
68
ASTM D2240
Tensile Strength, Yield 26.0 MPa
3770 psi
ASTM D638
Elongation at Break >= 900 %
>= 900 %
ASTM D638
Flexural Modulus 1.30 GPa
189 ksi
ASTM D790
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
ASTM D256
Thermal Properties Metric English Comments
Thermal Conductivity 0.480 W/m-K
3.33 BTU-in/hr-ft²-°F
ASTM D177
Vicat Softening Point 120 °C
248 °F
ASTM D1525
Processing Properties Metric English Comments
Melt Temperature 132 °C
270 °F
Copyright © lookpolymers.com All Rights Reserved