Iran Petrochemical (PCC) 60507 High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) 60507 High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
60507 is a HDPE injection molding grade which combines good flowability with balanced physical properties. This resin is well suited for general purpose applications requiring high stiffness. Application: crates, injection molding.Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.958 g/cc
0.0346 lb/in³
ASTM D1505
Melt Flow 7.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
7.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 13.0 MPa
1890 psi
ASTM D638
Tensile Strength, Yield 30.0 MPa
4350 psi
ASTM D638
Elongation at Break 350 %
350 %
ASTM D638
Flexural Modulus 1.50 GPa
218 ksi
ASTM D790
Izod Impact, Notched 0.360 J/cm
0.674 ft-lb/in
ASTM D256/A
Thermal Properties Metric English Comments
Vicat Softening Point 127 °C
261 °F
ASTM D1525