Intercontinental Polymers Deniers 1.5-2 Polyester Staple Fibers, Deniers 1.5 - 2

Category Polymer , Thermoplastic , Polyester, TP
Manufacturer Intercontinental Polymers, Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Intercontinental Polymers Deniers 1.5-2 Polyester Staple Fibers, Deniers 1.5 - 2.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Cut Lengths (Inches): 1, 1.25, 1.75, 2, 3 & 4. Lusters: Bright and Semi-Dull. Cross-Section: Round. Specialties: Optical Black, Spun-Dyed Black, Flame Retardant (US and European Standards), Cationic Dyeable, Hydrophobic, Hydrophilic, Trilobal and Hollow Cross-Section. Information provided by Intercontinental Polymers.
Mechanical Properties Metric English Comments
Elongation at Break 45 - 55 %
45 - 55 %
Tenacity 0.388 - 0.424 N/tex
4.40 - 4.80 g/denier
Thermal Properties Metric English Comments
Shrinkage 6.0 - 9.0 %
6.0 - 9.0 %
Hot Air Shrinkage
Descriptive Properties Value Comments
Crimp/Inch 11 - 15