Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Inno-Comp INNOPOL® CS 2-4630 GFR Flame Retarded Polypropylene Block-Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Flame Retardant
Manufacturer Inno-Comp Ltd
Trade Name INNOPOL® CS
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Inno-Comp INNOPOL® CS 2-4630 GFR Flame Retarded Polypropylene Block-Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
INNOPOL® CS 2-4630 GFR is a flame retarded polypropylene block-copolymer compound. This grade is available in nature and custom colored form.INNOPOL® CS 2-4630 GFR is recommended for producing injection molded products, where the required properties are excellent flame retardancy (V0) besides balanced physical properties.All information provided by INNO-COMP.
Physical Properties Metric English Comments
Density 0.950 g/cc

@Temperature 23.0 °C
0.0343 lb/in³

@Temperature 73.4 °F
ISO 1183
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 23.0 MPa
3340 psi
50 mm/min; ISO 527-1,-2
Elongation at Yield 5.0 %
5.0 %
50 mm/min; ISO 527-1,-2
Tensile Modulus 1.30 GPa
189 ksi
2 mm/min; ISO 527-1,-2
Flexural Modulus 1.45 GPa
210 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 3.50 kJ/m²

@Temperature -20.0 °C
1.67 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
5.00 kJ/m²

@Temperature 23.0 °C
2.38 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
ISO 75-1,-2
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
FMVSS 302
Descriptive Properties Value Comments
Automotive Materials Pass
FMVSS 302
Color Grey
Users viewing this material also viewed the following: