Inno-Comp INNOBATCH® PPH 6160 60% Talc-Filled Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Talc Filler
Manufacturer Inno-Comp Ltd
Trade Name INNOBATCH® PPH
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Inno-Comp INNOBATCH® PPH 6160 60% Talc-Filled Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
INNOBATCH® PPH 6160 is an 60% talc-filled polypropylene homopolymer based masterbatch. This grade is available in nature form.These products that are offered under the brand name INNOBATCH® are recommended for the area of packaging materials, but they can be used for manufacturing household appliances and outdoor furniture and for other purposes as well. The raw material having filler content is a semi-finished product from a user point of view; this allows the user to determine the optimal feeding rate during the processing operation.All information provided by INNO-COMP.
Physical Properties Metric English Comments
Density 1.50 g/cc

@Temperature 23.0 °C
0.0542 lb/in³

@Temperature 73.4 °F
ISO 1183
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Ash 53 - 63 %

@Temperature 600 °C
53 - 63 %

@Temperature 1110 °F
ISO 3451-1/A
Descriptive Properties Value Comments
Color Natural