Ineos T50-4400 HDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos T50-4400 HDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ineos T50-4400 is a high-flow high density polyethylene copolymer intended for injection molding of thin wall containers. This material will allow for cycle time reduction while still imparting reasonable impact strength. This resin meets the Food and Drug Administration requirements of 21CFR 177.1520.
Physical Properties Metric English Comments
Density 0.951 g/cc
0.0344 lb/in³
ASTM D4883
Melt Flow 47 g/10 min

@Load 2.16 kg,
Temperature 190 °C
47 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength, Yield 25.5 MPa
3700 psi
2 in/min (50 mm/min); ASTM D-638
Flexural Modulus 1.207 GPa
175.1 ksi
Tangent-Method 1; ASTM D790
Izod Impact, Notched 0.200 J/cm
0.375 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 74.0 °C
165 °F
ASTM D648
Vicat Softening Point 120 °C
248 °F
ASTM D1525
Brittleness Temperature <= -75.0 °C
<= -103 °F
ASTM D746
Descriptive Properties Value Comments
Process Injection Molding
Region US & Canada
Bamberger Polymers Distribution