Material Notes:
High heat, easy flow general purpose polystyrene with excellent clarity. Designed for applications requiring a combination of fast processing with good strength and heat resistance.Information provided by BASF.Ineos Styrenics purchased this product line from BASF in 2005.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
ASTM D955
Melt Flow 6.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
6.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 44.0 MPa
6380 psi
Elongation at Break 2.0 %
2.0 %
Tensile Modulus 2.48 GPa
360 ksi
Flexural Modulus 3.10 GPa
450 ksi
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 88.0 °C
190 °F
Vicat Softening Point 109 °C
228 °F
Flammability, UL94 HB

@Thickness 1.47 mm
HB

@Thickness 0.0579 in
Processing Properties Metric English Comments
Melt Temperature 200 - 230 °C
392 - 446 °F
Extrusion
180 - 280 °C
356 - 536 °F
Molding