Ineos Styrenics 166H General Purpose Polystyrene (NAFTA)

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Molded, Unreinforced
Manufacturer Ineos Styrenics
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos Styrenics 166H General Purpose Polystyrene (NAFTA).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Polystyrene 166H is a high molecular weight general purpose polystyrene with good flow and crystal clarity. Polystyrene 166H offers good processing characteristics while yielding parts with exceptional toughness relative to standard GPPS.Information provided by BASF.Ineos Styrenics purchased this product line from BASF in 2005.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
ASTM D955
Melt Flow 3.6 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.6 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 77
77
ASTM D785
Tensile Strength at Break 41.0 MPa
5950 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Tensile Modulus 2.41 GPa
350 ksi
ASTM D638
Flexural Modulus 3.05 GPa
442 ksi
ASTM D790-1
Izod Impact, Notched 0.160 J/cm
0.300 ft-lb/in
ASTM D256-A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
ASTM D648
Vicat Softening Point 98.0 °C
208 °F
ASTM D1525
Flammability, UL94 HB

@Thickness 1.47 mm
HB

@Thickness 0.0579 in
All Colors
Processing Properties Metric English Comments
Melt Temperature 200 - 230 °C
392 - 446 °F
Extrusion
180 - 280 °C
356 - 536 °F
Molding