Material Notes:
Description: High-heat, high-molecular weight grades for a variety of applications, including medical devices and labware, cosmetics packaging, CD & DVD jewel boxes, food serviceware, and low-taste, low-odor products such as cook and cake trays as well as other oriented polystyrene (OPS) applications.Information provided by BASF.Ineos Styrenics purchased this product line from BASF in 2005.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
ASTM D955
Melt Flow 3.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 76
76
ASTM D785
Tensile Strength at Break 49.0 MPa
7110 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Tensile Modulus 2.52 GPa
366 ksi
ASTM D638
Flexural Modulus 3.24 GPa
470 ksi
ASTM D790-1
Izod Impact, Notched 0.160 J/cm
0.300 ft-lb/in
ASTM D256-A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 94.0 °C
201 °F
ASTM D648
Vicat Softening Point 109 °C
228 °F
ASTM D1525
Flammability, UL94 HB

@Thickness 1.47 mm
HB

@Thickness 0.0579 in
All Colors
Processing Properties Metric English Comments
Melt Temperature 210 - 240 °C
410 - 464 °F
Extrusion
180 - 280 °C
356 - 536 °F
Molding