Ineos Nova S-4122 Medium Impact Compact Polystyrene  (discontinued **)

Category Polymer , Thermoplastic , Polystyrene (PS)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos Nova S-4122 Medium Impact Compact Polystyrene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Low friction, medium impact polystyrene which combines excellent flow characteristics with a good dimensional stability under heat and a high stiffness. This grade is designed for injection molding of technical parts.All mechanical properties measured under standard conditions 50% RH and 23°C.Information provided by NOVA Chemicals.INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture between NOVA Chemicals and INEOS to include North American assets. 
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
DIN 53479
Water Absorption <= 0.10 %
<= 0.10 %
DIN 53495
Melt Flow 7.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
7.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
DIN 5375/ISO 1133
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
DIN 53453/ISO 179
Thermal Properties Metric English Comments
CTE, linear 80.0 µm/m-°C

@Temperature 20.0 °C
44.4 µin/in-°F

@Temperature 68.0 °F
DIN 53752
Thermal Conductivity 0.160 W/m-K
1.11 BTU-in/hr-ft²-°F
DIN 52612
Vicat Softening Point 92.0 °C
198 °F
DIN 53460
Users viewing this material also viewed the following: