Ineos Nova 8048 High Performance Styrenic Enhanced Polystyrene  (discontinued **)

Category Polymer , Thermoplastic , Polystyrene (PS)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos Nova 8048 High Performance Styrenic Enhanced Polystyrene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Improved toughness, Custom colorsApplications: Designed for injection molding applications requiring clarity and toughnessPerformance grades of polystyrene are engineered to have specific properties. These products can be custom colored. NOVA Chemicals can accurately match your color needs with its leading edge color technology. Injection Speed: FastColored material may differ in some properties. All molded samples were an 1/8 inch thick unless noted.Information provided by NOVA Chemicals.INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture between NOVA Chemicals and INEOS to include North American assets. 
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D955
Melt Flow 14 g/10 min

@Load 5.00 kg,
Temperature 200 °C
14 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 41.0 MPa
5950 psi
2.0 in/min; ASTM D638
Elongation at Break 3.0 %
3.0 %
2.0 in/min; ASTM D638
Flexural Strength 59.0 MPa
8560 psi
0.1 in/min; ASTM D790
Flexural Modulus 2.76 GPa
400 ksi
0.1 in/min; ASTM D790
Izod Impact, Notched 0.200 J/cm
0.375 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
ASTM D648
Vicat Softening Point 95.0 °C
203 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature <= 260 °C
<= 500 °F
Rear Barrel Temperature 177 - 199 °C
351 - 390 °F
Middle Barrel Temperature 193 - 216 °C
379 - 421 °F
Front Barrel Temperature 199 - 221 °C
390 - 430 °F
Melt Temperature 204 - 227 °C
399 - 441 °F
Mold Temperature 27.0 - 54.0 °C
80.6 - 129 °F
Drying Temperature 68.0 °C
154 °F
Dry Time 2 hour
2 hour
Back Pressure 0.345 MPa
50.0 psi
Copyright © lookpolymers.com All Rights Reserved