Ineos Nova 610 Crystal Polystyrene GP Grade  (discontinued **)

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Transparent Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos Nova 610 Crystal Polystyrene GP Grade  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Broad, medium melt flow range, Broad Vicat rangeApplications: Any; Injection Molding and ExtrusionProperties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwise specified.Information provided by NOVA Chemicals.INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture between NOVA Chemicals and INEOS to include North American assets. 
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ISO 1183A
Melt Flow 3.8 - 5.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.8 - 5.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.200 J/cm

@Diameter 3.17 mm
0.375 ft-lb/in

@Diameter 0.125 in
bar, 0.010" notch radius; ISO 180
Thermal Properties Metric English Comments
Vicat Softening Point 88.0 - 106 °C
190 - 223 °F
ISO 306A
Electrical Properties Metric English Comments
Dielectric Constant 2.59

@Frequency 1e+6 Hz
2.59

@Frequency 1e+6 Hz
Dielectric Strength 19.7 kV/mm

@Thickness 3.17 mm
500 kV/in

@Thickness 0.125 in
Processing Properties Metric English Comments
Melt Temperature 190 - 274 °C
374 - 525 °F
Mold Temperature 10.0 - 60.0 °C
50.0 - 140 °F