Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ineos N10N-00 Polypropylene Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos N10N-00 Polypropylene Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Grade N10N-00 is a nucleated polypropylene impact copolymer with an excellent balance of stiffness and impact resistance for injection molding applications and compounding products used in Lawn and Garden applications. It has good stiffness and excellent impact resistance even at sub ambient temperature. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520
Physical Properties Metric English Comments
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 230 °C
10 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 71.8
71.8
Tensile Strength, Yield 23.6 MPa
3430 psi
ASTM D638
Elongation at Yield 6.0 %
6.0 %
ASTM D638
Tensile Modulus 1.32 GPa
191 ksi
Tangent Method; ASTM D638
Flexural Modulus, 1% Secant 1100 MPa
160000 psi
0.05"/min test speed; ASTM D790A
Izod Impact, Notched 1.01 J/cm

@Temperature -20.0 °C
1.90 ft-lb/in

@Temperature -4.00 °F
1/8" (3mm) notched bar; ASTM D256
6.03 J/cm

@Temperature 23.0 °C
11.3 ft-lb/in

@Temperature 73.4 °F
1/8" (3mm) notched bar; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 92.28 °C
198.1 °F
ASTM D648
Optical Properties Metric English Comments
Gloss 64.5 %
64.5 %
at 60° angle; ASTM D523