Ineos L24G-00 Polypropylene Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos L24G-00 Polypropylene Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Grade L24G-00 is a high melt flow rate, antistatic high impact copolymer polypropylene for injection molding applications. It offers excellent impact resistance and a high flexural modulus. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.ApplicationsConsumer products Housewares AutomotiveBenefitsHigh impact resistance High flexural modulus
Physical Properties Metric English Comments
Melt Flow 24 g/10 min

@Load 2.16 kg,
Temperature 230 °C
24 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 75
75
ASTM D785
Tensile Strength, Yield 24.8 MPa
3600 psi
ASTM D638
Elongation at Break >= 200 %
>= 200 %
ASTM D638
Flexural Modulus 1.17 GPa
170 ksi
ASTM D790B
Izod Impact, Notched 1.60 J/cm

@Diameter 3.17 mm
3.00 ft-lb/in

@Diameter 0.125 in
bar; ASTM D256
0.481 J/cm

@Diameter 3.00 mm,
Temperature -20.0 °C
0.900 ft-lb/in

@Diameter 0.118 in,
Temperature -4.00 °F
bar; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 87.8 °C
190 °F
ASTM D648
Descriptive Properties Value Comments
Process Injection Molding