Material Notes:
L10G-00 is a barefoot polypropylene impact copolymer designed for injection molding applications. It offers excellent impact resistance, high flexural modulus and good processability. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.ApplicationsInjection moldingConsumer productsBenefitsHigh impact resistanceHigh flexural modulusInformation provided by Ineos Olefins & Polymers USA
Physical Properties Metric English Comments
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 230 °C
10 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 27.5 MPa
3990 psi
ASTM D638
Flexural Modulus 1.13 GPa
164 ksi
ASTM D790A
Izod Impact, Notched 0.908 J/cm
1.70 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 87.0 °C
189 °F
ASTM D648
Descriptive Properties Value Comments
Process Injection Molding
Users viewing this material also viewed the following: