Ineos K54-05 HDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos K54-05 HDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
K54-05 is a high molecular weight, high density polyethylene copolymer developed for large-part blow molding (drum market) where the finished product demands outstanding physical performance. This material combines excellent processability and environmental stress crack resistance (ESCR) with superior impact and other well-balanced end use properties. This resin meets the Food and Drug Administration requirements of 21CFR 177.1520 for contact with food.
Physical Properties Metric English Comments
Density 0.954 g/cc
0.0345 lb/in³
ASTM D4883
High Load Melt Index 5.0 g/10 min
5.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 64
64
ASTM D2240
Tensile Strength, Yield 27.0 MPa
3920 psi
2 in/min (50 mm/min); ASTM D638
Elongation at Break 900 %
900 %
2 in/min (50 mm/min); ASTM D638
Flexural Modulus 1.241 GPa
180.0 ksi
Tangent; ASTM D 570
Izod Impact, Notched 8.50 J/cm
15.9 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 76.0 °C
169 °F
ASTM D648
Vicat Softening Point 132 °C
270 °F
ASTM D1525
Brittleness Temperature <= -75.0 °C
<= -103 °F
ASTM D746
Descriptive Properties Value Comments
Process Blow Molding
Region US & Canada
Bamberger Polymers Distribution