Material Notes:
J60-1700-173 is a high density polyethylene homopolymer. This resin is a product of Ineos' technology and is characterized by a narrow molecular weight distribution. Parts fabricated from this material exhibit excellent gloss and rigidity. This material meets the Food and Drug Administration requirements of 21CFR 177.1520.
Physical Properties Metric English Comments
Density 0.961 g/cc
0.0347 lb/in³
ASTM D4883
Melt Flow 16 g/10 min

@Load 2.16 kg,
Temperature 190 °C
16 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength, Yield 31.0 MPa
4500 psi
2 in/min (50 mm/min); ASTM D-638
Flexural Modulus 1.552 GPa
225.1 ksi
Tangent; ASTM D 790
Izod Impact, Notched 0.380 J/cm
0.712 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 81.0 °C
178 °F
ASTM D648
Vicat Softening Point 127 °C
261 °F
ASTM D1525
Brittleness Temperature <= -75.0 °C
<= -103 °F
ASTM D746
Descriptive Properties Value Comments
Process Injection Molding
Region US & Canada
Bamberger Polymers Distribution