Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ineos H35Z-00 Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos H35Z-00 Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This is a high flow rate, nucleated and antistatic homopolymer for injection molding applications. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.ApplicationsConsumer productsHousewaresMedical componentsThin-wall rigid packagingBenefitsHigh flow rateFast cycle timesGood molding performance in thin-walled partsLow static chargeImproved toughnessInformation provided by Ineos Olefins & Polymers USA
Physical Properties Metric English Comments
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 38.6 MPa

@Temperature 23.0 °C
5600 psi

@Temperature 73.4 °F
ASTM D638
Elongation at Break 30 %
30 %
ASTM D638
Elongation at Yield 8.0 %
8.0 %
ASTM D638
Flexural Modulus 1.65 GPa

@Temperature 23.0 °C
240 ksi

@Temperature 73.4 °F
ASTM D790A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 121 °C
250 °F
ASTM D648
Descriptive Properties Value Comments
Process Injection Molding
Region Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution
Copyright © lookpolymers.com All Rights Reserved