Material Notes:
Grade H12G-01 is a general purpose homopolymer. This material meets the requirements of the US Food and Drug Administration as specified in 21 CFR 177.1520 for use in food-contact applications for food type Categories I through IX of Table 1, under conditions of use A through H of Table 2 in Title 21 CFR, Part 176.170(c).Applications:General Purpose Injection and ExtrusionHousewaresRigid PackagingCaps & ClosuresFilm and SheetInformation provided by Ineos Olefins & Polymers USA
Physical Properties Metric English Comments
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 76
76
ASTM D2240
Tensile Strength at Break 13.8 MPa
2000 psi
2 in/min; ASTM D638
Tensile Strength, Yield 35.9 MPa
5200 psi
2 in/min; ASTM D638
Elongation at Break >= 250 %
>= 250 %
2 in/min; ASTM D638
Elongation at Yield 11 %
11 %
2 in/min; ASTM D638
Flexural Modulus 1.48 GPa
215 ksi
1% Secant, 0.05 in/min; ASTM D790A
Izod Impact, Notched 0.315 J/cm
0.590 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
ASTM D648
Descriptive Properties Value Comments
Process Extrusion
Injection Molding
Region Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following: